Plasma enhanced atomic layer deposition of silicon nitride using magnetized very high frequency plasma

  • You Jin Ji
  • , Hae In Kim
  • , Ji Eun Kang
  • , Seung Yup Choi
  • , Ki Hyun Kim
  • , Doo San Kim
  • , A. R. Ellingboe
  • , Hye Min Kim
  • , Geun Young Yeom
  • , Dong Woo Kim
  • Sungkyunkwan University
  • University of Texas at Dallas
  • Dublin City University
  • Korea Maritime and Ocean University

Research output: Contribution to journal › Article › peer-review

Abstract

To obtain high-quality SiNx films applicable to an extensive range of processes, such as gate spacers in fin field-effect transistors (FinFETs), the self-aligned quadruple patterning process, etc, a study of plasma with higher plasma density and lower plasma damage is crucial in addition to study on novel precursors for SiN x plasma-enhanced atomic layer deposition (PEALD) processes. In this study, a novel magnetized PEALD process was developed for depositing high-quality SiNx films using di(isopropylamino)silane (DIPAS) and magnetized N2 plasma at a low substrate temperature of 200 °C. The properties of the deposited SiNx films were analyzed and compared with those obtained by the PEALD process using a non-magnetized N2 plasma source under the same conditions. The PEALD SiNx film, produced using an external magnetic field (ranging from 0 to 100 G) during the plasma exposure step, exhibited a higher growth rate (∼1 Å/cycle) due to the increased plasma density. Additionally, it showed lower surface roughness, higher film density, and enhanced wet etch resistance compared to films deposited using the PEALD process with non-magnetized plasmas. This improvement can be attributed to the higher ion flux and lower ion energy of the magnetized plasma. The electrical characteristics, such as interface trap density and breakdown voltage, were also enhanced when the magnetized plasma was used for the PEALD process. Furthermore, when SiNx films were deposited on high-aspect-ratio (30:1) trench patterns using the magnetized PEALD process, an improved step coverage of over 98% was achieved, in contrast to the conformality of SiNx deposited using non-magnetized plasma. This enhancement is possibly a result of deeper radical penetration enabled by the magnetized plasma.

Original languageEnglish
Article number275701
JournalNanotechnology
Volume35
Issue number27
DOIs
StatePublished - 1 Jul 2024

Keywords

  • di(isopropylamino)silane
  • DIPAS
  • magnetized plasma
  • N plasma
  • plasma enhanced atomic layer deposition
  • silicon nitride