Skip to main navigation Skip to search Skip to main content

Dependence of etch rates of silicon substrates on the use of C4 F8 and C4 F6 plasmas in the deposition step of the Bosch process

  • Hyongmoo Rhee
  • , Hae Min Lee
  • , Yun Mi Namkoung
  • , Chang Koo Kim
  • , Heeyeop Chae
  • , Yil Wook Kim
  • Ajou University
  • Eugene Technology Co., Ltd.

Research output: Contribution to journal › Article › peer-review

Abstract

The Bosch process was carried out using S F6 C4 F8 or S F6 C4 F6 plasmas during the etching/deposition steps to examine the etch profiles and etch rates of silicon. The fluorocarbon film deposited in a C4 F6 plasma was thicker and more strongly bonded than the film deposited in a C4 F8 plasma, which led to a shorter deposition time for the C4 F6 plasma. The deposition rate of the fluorocarbon films on the different locations of the silicon substrate in both C4 F8 and C4 F6 plasmas decreased in the following order: top≥bottom≥ sidewall. However, the normalized deposition rate of the bottom surface with respect to the top surface was higher for the C4 F8 plasma (0.92) than for the C4 F6 plasma (0.65), indicating that a thicker fluorocarbon film was deposited at the bottom of the pattern in C4 F8 plasma under the same process conditions. This resulted in a higher etch rate of the silicon substrate using C4 F6 plasma during the deposition step of the Bosch process, even though a fluorocarbon film with a similar thickness had been deposited on the top surface for both C4 F8 and C4 F6 plasmas.

Original languageEnglish
Pages (from-to)33-40
Number of pages8
JournalJournal of Vacuum Science and Technology B: Microelectronics and Nanometer Structures
Volume27
Issue number1
DOIs
StatePublished - 2009

Fingerprint

Dive into the research topics of 'Dependence of etch rates of silicon substrates on the use of C4 F8 and C4 F6 plasmas in the deposition step of the Bosch process'. Together they form a unique fingerprint.