Atomic layer deposition of thin-film ceramic electrolytes for high-performance fuel cells

  • Joon Hyung Shim
  • , Sangkyun Kang
  • , Suk Won Cha
  • , Wonyoung Lee
  • , Young Beom Kim
  • , Joong Sun Park
  • , Turgut M. Gür
  • , Fritz B. Prinz
  • , Cheng Chieh Chao
  • , Jihwan An
  • Korea University
  • Hanchang Ind. Co. Ltd.
  • Seoul National University
  • Hanyang University
  • Lawrence Berkeley National Laboratory
  • Stanford University

Research output: Contribution to journalArticlepeer-review

Abstract

This feature article provides a progress review of atomic layer deposition (ALD) for fabrication of oxide-ion as well as proton conducting ceramic fuel cells. A comprehensive analysis of structural, chemical, surface kinetics, and electrochemical characterization results of ALD membranes is also presented. ALD is a surface reaction limited method of depositing conformal, high quality, pinhole-free, uniform thickness nanofilms onto planar or three-dimensional structures. Deposition by one atomic layer at a time also affords unprecedented opportunities to engineer surface termination, to form compositionally graded structures or graded doping, and to synthesize metastable phases that cannot be realized otherwise. Indeed, thin ceramic electrolyte membranes made by ALD exhibit enhanced surface exchange kinetics, reduced ohmic losses, and superior fuel cell performance as high as 1.34 W cm-2 at 500 °C. More importantly, ALD offers the opportunity to design and engineer surface structures at the atomic scale targeting improved performance of not only ceramic fuel cells, but also electrochemical sensors, electrolysers and pumps.

Original languageEnglish
Pages (from-to)12695-12705
Number of pages11
JournalJournal of Materials Chemistry A
Volume1
Issue number41
DOIs
StatePublished - 7 Nov 2013

UN SDGs

This output contributes to the following UN Sustainable Development Goals (SDGs)

  1. SDG 7 - Affordable and Clean Energy
    SDG 7 Affordable and Clean Energy

Fingerprint

Dive into the research topics of 'Atomic layer deposition of thin-film ceramic electrolytes for high-performance fuel cells'. Together they form a unique fingerprint.

Cite this