Area selective atomic layer deposition by soft lithography

  • Rong Chen
  • , David W. Porter
  • , Hyoungsub Kim
  • , Paul C. Mcintyre
  • , Stacey F. Bent
  • Stanford University

Research output: Chapter in Book/Report/Conference proceeding › Conference contribution › peer-review

Abstract

Area selective HfO2 thin film growth through atomic layer deposition (ALD) has been achieved on octadecyltrichlorosilane (ODTS) patterned Si substrates. Patterned hydrophobic self-assembled monolayers (SAMs) were first transferred to Si substrates by micro-contact printing. Using hafnium-tetrachloride or tetrakis(dimethylamido) hafnium(IV) and water as ALD precursors, amorphous HfO2 layers were then grown selectively on the SAM-free regions of the surface where native hydroxyl groups nucleate growth from the vapor phase. The HfO2 pattern was readily observed through scanning electron microscopy and scanning Auger imaging, demonstrating that soft lithography is a simple and promising method to achieve area selective ALD. To evaluate the selectivity, the resolution of the soft lithography based method was compared with that of area selective ALD of HfO2 by selective surface modification of patterned silicon oxide obtained using long-time SAM exposure. It was found that the selective surface modification showed much higher spatial resolution and selectivity, an observation consistent with previous studies indicating that highly ordered and densely packed ODTS films were important to achieve complete deactivation.

Original languageEnglish
Title of host publicationGate Stack Scaling
Subtitle of host publicationMaterials Selection, Role of Interfaces, and Reliability Implications
PublisherMaterials Research Society
Pages161-166
Number of pages6
ISBN (Print)1558998748, 9781558998742
DOIs
StatePublished - 2006
Event2006 MRS Spring Meeting - San Francisco, CA, United States
Duration: 18 Apr 2006 → 19 Apr 2006

Publication series

NameMaterials Research Society Symposium Proceedings
Volume917
ISSN (Print)0272-9172

Conference

Conference2006 MRS Spring Meeting
Country/TerritoryUnited States
CitySan Francisco, CA
Period18/04/06 → 19/04/06

Fingerprint

Dive into the research topics of 'Area selective atomic layer deposition by soft lithography'. Together they form a unique fingerprint.

Cite this