Amidoxime-Containing Zr and Hf Atomic Layer Deposition Precursors for Metal Oxide Thin Films

  • Ga Yeon Lee
  • , Seung Hun Lee
  • , In Ho Jo
  • , Chan Mi Cho
  • , Svetlana Shostak
  • , Ji Yeon Ryu
  • , Bo Keun Park
  • , Seung Uk Son
  • , Cheol Ho Choi
  • , Taeyong Eom
  • , Jeong Hwan Kim
  • , Taek Mo Chung
  • Korea Research Institute of Chemical Technology
  • Hanbat National University
  • Kyungpook National University
  • University of Science and Technology UST

Research output: Contribution to journalArticlepeer-review

Abstract

In this article, we discuss the synthesis of eight novel zirconium and hafnium complexes containing amidoxime ligands as potential precursors for atomic layer deposition (ALD). Two amidoximes, viz., (E)-N′-hydroxy-N,N-dimethylacetimidamide (mdaoH) and (Z)-N′-hydroxy-N,N-dimethylpivalimidamide (tdaoH), along with their Zr and Hf homoleptic complexes, Zr(mdao)4 (1), Hf(mdao)4 (2), Zr(tdao)4 (3), and Hf(tdao)4 (4) were prepared. We further synthesized heteroleptic compounds with different physical properties by introducing cyclopentadienyl (Cp) ligand, namely, CpZr(mdao)3 (5), CpHf(mdao)3 (6), CpZr(tdao)3 (7), and CpHf(tdao)3 (8). Thermogravimetric analysis was used for the assessment of the evaporation characteristics of complexes 1, 2, 5, and 6, and it revealed multistep weight losses with high residues. On the other hand, the thermogravimetric analysis curves of complexes 3, 4, 7, and 8 comprising tdao ligands revealed single-step weight losses with moderate residues. Single-crystal X-ray diffraction studies of complexes 1, 3, and 7 showed that all of the complexes have monomeric molecular structures. Complex 7 exhibited a low melting point (75 °C), good volatility, and high thermal stability compared with other complexes. Therefore, an atomic layer deposition process for the growth of ZrO2 was developed by using ZrCp(tdao)3 (7) as a novel precursor.

Original languageEnglish
Pages (from-to)537-547
Number of pages11
JournalInorganic Chemistry
Volume63
Issue number1
DOIs
StatePublished - 8 Jan 2024

Fingerprint

Dive into the research topics of 'Amidoxime-Containing Zr and Hf Atomic Layer Deposition Precursors for Metal Oxide Thin Films'. Together they form a unique fingerprint.